Rhonda’s Terra Sigillata Base
Firing Temperature: Cone 04-10
Atmosphere: Reduction, Oxidation
Surface Finish: Satin
Color: White, Black, Various, Blue
Rhonda’s Blue/Black Terra Sigillata
Firing Temperature: Cone 04-10
Atmosphere: Oxidation
Surface Finish: Satin
Color: Black, Blue
Slate Blue
Firing Temperature: Cone 6
Atmosphere: Reduction
Surface Finish: Glossy to satin
Color: Blue
Blue Low-Fire Glaze
Firing Temperature: Cone 04
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Glossy
Color: Blue
Amber Ash
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation/Neutral
Color: Various, Blue
Cowan Amber
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Satin to glossy
Color: Various
Cowan Amber Ash Glaze
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Satin to glossy
Color: Various
Basic Ash Recipe
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Satin to glossy
Color: Various
Zack’s Black
Firing Temperature: Cone 9-11
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Satin
Color: Black
Semi-Matte Black
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Satin matte
Color: Black