Sapphire Blue Jewel Base Glaze
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Dark blue
Bright Glaze I (plum)
Firing Temperature: Cone 06
Atmosphere: Oxidation/Neutral
Surface Finish: Matte
Color: Dark purple
Val’s Satin Black Glaze (Variation)
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Satin matte
Color: Black
Beth’s Blue
Firing Temperature: Cone 9, Cone 11
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Dark blue
Turner’s White + CoCO3 and Li2CO3 in Reduction
Firing Temperature: Cone 6-10
Atmosphere: Reduction
Surface Finish: Matte
Color: Medium purple
Turner’s White + CoCO3 and Li2CO3
Firing Temperature: Cone 6-10
Atmosphere: Oxidation/Neutral
Surface Finish: Matte
Color: Medium purple
Textured Blue
Firing Temperature: Cone 6
Atmosphere: Reduction
Surface Finish: Textured
Color: Medium blue
Matt Glaze – Blue
Firing Temperature: Cone 06
Atmosphere: Oxidation/Neutral
Surface Finish: Matte
Color: Cobalt blue
Martin’s Moveable Feast – Persian Blue
Firing Temperature: Cone 10
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Medium blue
Martin’s Moveable Feast – Orchard Purple
Firing Temperature: Cone 10
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Dark purple