Matte Flux Variation (1-B2-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Blue
Matte Flux Variation (1-B1-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy to satin
Color: Blue
Oatmeal Variation (1-B4-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Satin
Color: Blue
Oatmeal Variation (1-B3-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Matte to satin
Color: Blue
Oatmeal Variation (1-B2-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy to satin
Color: Blue
Oatmeal Variation (1-B1-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Satin
Color: Blue
Cream Cheese Matte Glaze with Cobalt Carbonate
Firing Temperature: Cone 4-6
Atmosphere: Oxidation
Surface Finish: Satin
Color: Blue
Dry Sandstone Base Glaze—Seldom Seen Blue-Green
Firing Temperature: Cone 4-6
Atmosphere: Oxidation
Surface Finish: Satin
Color: Green
Dry Sandstone Base Glaze—I Like That Blue
Firing Temperature: Cone 4-6
Atmosphere: Oxidation
Surface Finish: Satin
Color: Blue
Dry Sandstone Base Glaze with Cobalt Carbonate, Red Iron Oxide, and Titanium Dioxide
Firing Temperature: Cone 4-6
Atmosphere: Oxidation
Surface Finish: Satin
Color: Green