Firing Temperature: Cone 04-2

Atmosphere: Oxidation

Surface Finish: Satin

Color: White, Red

Terra Sigillata Base

Terra Sigillata Base

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 03

Atmosphere: Oxidation

Surface Finish: Matte to satin

Color: White

Terra Sigillata Base Recipe

Terra Sigillata Base Recipe

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04-2

Atmosphere: Oxidation

Surface Finish: Satin

Color: White, Gray, Yellow green, Turquoise, Yellow