Black Stain

Black Stain

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Color: Black

John Solly Chrome Green Glaze for Earthenware

John Solly Chrome Green Glaze for Earthenware

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Medium green