Recipe Tags: Chromium Oxide

Flux Saturation (4-H4-O6)

Flux Saturation (4-H4-O6)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Satin matte

Color: Yellow

Flux Saturation (4-H3-O6)

Flux Saturation (4-H3-O6)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Satin

Color: Yellow

Shiny Flux Variation (4-H3-R9)

Shiny Flux Variation (4-H3-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Satin

Color: Brown

Ruby

Ruby

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation/Neutral

Surface Finish: Glossy

Color: Ruby

Emerald

Emerald

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation/Neutral

Surface Finish: Glossy

Color: Emerald

Green Egyptian Paste

Green Egyptian Paste

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 016

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Light green

Chrome-Tin Red

Chrome-Tin Red

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Dark red

Chrome-Tin Maroon

Chrome-Tin Maroon

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Dark red

Chrome Green Runny Transparent for Stoneware

Chrome Green Runny Transparent for Stoneware

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation/Neutral

Surface Finish: Glossy

Color: Dark green