Sprite Bottle Green 04
Firing Temperature: Cone 04-03
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Green
Chris Clear
Firing Temperature: Cone 01-05
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear, Turquoise, Green, Blue
Green Apple
Firing Temperature: Cone 6-7
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Light green, Yellow green
Val’s Satin Black
Firing Temperature: Cone 9-12
Atmosphere: Reduction
Surface Finish: Satin
Color: Black
Faux Lead Hulk Smash Green
Firing Temperature: Cone 04
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Green
Metallic Black
Firing Temperature: Cone 6
Atmosphere: Oxidation/Neutral
Surface Finish: Satin matte, Matte to satin
Color: Black
Cary’s Crystal Glaze – Crystal Yellow Green
Firing Temperature: Cone 02
Atmosphere: Oxidation/Neutral
Surface Finish: Textured
Color: Yellow green
Deb’s Teal Clear Base
Firing Temperature: Cone 04
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Teal
Flat Matte Black
Firing Temperature: Cone 10
Atmosphere: Oxidation/Neutral
Surface Finish: Matte
Color: Black
Burgundy/Red
Firing Temperature: Cone 6
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Dark red