Tan-Yellow Transparent

Tan-Yellow Transparent

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Oxidation

Color: Medium tan, Light tan, Yellow

Barium Yellow Matte

Barium Yellow Matte

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6-8

Surface Finish: Matte

Color: Tan, Yellow

Iron Honey Yellow

Iron Honey Yellow

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Oxidation

Surface Finish: Glossy

Color: Yellow

Praseodymium-Zirconium Yellow

Praseodymium-Zirconium Yellow

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Oxidation

Surface Finish: Glossy

Color: Yellow

Cadmium Yellow Glaze

Cadmium Yellow Glaze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Oxidation

Surface Finish: Glossy

Color: Yellow

Chun Reduced

Chun Reduced

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Light blue

Sea Green Runny Transparent for Porcelain

Sea Green Runny Transparent for Porcelain

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6-8

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Turquoise green

Magnesium Matte Green for Stoneware

Magnesium Matte Green for Stoneware

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 8

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Light green

Iron Red

Iron Red

2 votes, average: 3.50 out of 52 votes, average: 3.50 out of 52 votes, average: 3.50 out of 52 votes, average: 3.50 out of 52 votes, average: 3.50 out of 5 (2 votes, average: 3.50 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6-8

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Dark red

HAA2

HAA2

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9-10

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: White