Recipe Tags: Calcium Carbonate

Matte Flux Variation (4-D4-R9)

Matte Flux Variation (4-D4-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Matte to satin

Color: Brown

Matte Flux Variation (4-D3-R9)

Matte Flux Variation (4-D3-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Color: Tan

Oatmeal Variation (1-D4-R9)

Oatmeal Variation (1-D4-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Satin

Color: Brown

Oatmeal Variation (1-D3-R9)

Oatmeal Variation (1-D3-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Satin

Color: Brown

Oatmeal Variation (1-D1-R9)

Oatmeal Variation (1-D1-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Color: Gray, Yellow

Oriental Iron Glaze (19-C1-R9)

Oriental Iron Glaze (19-C1-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy

Color: Red

Oriental Iron Glaze (19-C3-R9)

Oriental Iron Glaze (19-C3-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy

Color: Dark red

Oriental Iron Glaze (19-B4-R9)

Oriental Iron Glaze (19-B4-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy to satin

Color: Blue

Oriental Iron Glaze (19-B1-R9)

Oriental Iron Glaze (19-B1-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy

Color: Blue

Oriental Iron Glaze (11-B2-R9)

Oriental Iron Glaze (11-B2-R9)

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9

Atmosphere: Reduction

Surface Finish: Glossy

Color: Blue