Recipe Tags: Calcined Kaolin

Tony Hansen’s G2934—Silky Black

Tony Hansen’s G2934—Silky Black

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Satin

Color: Black

Tony Hansen’s G2934—Brown

Tony Hansen’s G2934—Brown

1 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 51 vote, average: 5.00 out of 5 (1 votes, average: 5.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Glossy

Color: Brown

Tony Hansen’s G2934—White

Tony Hansen’s G2934—White

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Glossy

Color: White

Tony Hansen’s G2934 Base Glaze

Tony Hansen’s G2934 Base Glaze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation

Surface Finish: Glossy

Color: Clear

White Engobe

White Engobe

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 06-02

Atmosphere: Oxidation

Surface Finish: Glossy to satin

Color: White

Engobe blue

Engobe blue

1 vote, average: 1.00 out of 51 vote, average: 1.00 out of 51 vote, average: 1.00 out of 51 vote, average: 1.00 out of 51 vote, average: 1.00 out of 5 (1 votes, average: 1.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 1–6

Atmosphere: Reduction, Oxidation/Neutral

Surface Finish: Matte

Color: Blue

Rhodes Crackle Slip

Rhodes Crackle Slip

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction

Surface Finish: Textured

Color: Light brown

Courtney’s Sugary Satin Clear

Courtney’s Sugary Satin Clear

2 votes, average: 2.00 out of 52 votes, average: 2.00 out of 52 votes, average: 2.00 out of 52 votes, average: 2.00 out of 52 votes, average: 2.00 out of 5 (2 votes, average: 2.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 02–03

Atmosphere: Oxidation/Neutral

Surface Finish: Satin matte

Color: Clear

Bristol Glaze IX

Bristol Glaze IX

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Light green