Recipe Tags: Calcined EPK Kaolin

Kiln Wash

Kiln Wash

1 vote, average: 4.00 out of 51 vote, average: 4.00 out of 51 vote, average: 4.00 out of 51 vote, average: 4.00 out of 51 vote, average: 4.00 out of 5 (1 votes, average: 4.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 07-10

Atmosphere: Reduction, Oxidation

Ostrom’s White Slip

Ostrom’s White Slip

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Oxidation/Neutral

Surface Finish: Satin matte

Color: White

Icy Blue Glaze

Icy Blue Glaze

4 votes, average: 4.25 out of 54 votes, average: 4.25 out of 54 votes, average: 4.25 out of 54 votes, average: 4.25 out of 54 votes, average: 4.25 out of 5 (4 votes, average: 4.25 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04

Atmosphere: Oxidation/Neutral

Surface Finish: Satin matte

Color: Turquoise blue