Miranda Thomas Jun Glaze
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Brown
Oribe Green
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Green, Blue
Oriental Iron Glaze (9-F4-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Matte to satin
Color: Medium green, Tan
Oriental Iron Glaze (30-A3-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Matte to satin
Color: Brown
Oriental Iron Glaze (32-A5-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Matte to satin
Color: Brown
Oriental Iron Glaze (31-A5-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy to satin
Color: Brown
Oriental Iron Glaze (32-A4-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy to satin
Color: Brown
Tomato Red Base (Tile 6)
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Glossy to satin
Color: Red
Nuka
Firing Temperature: Cone 11
Atmosphere: Reduction, Wood
Surface Finish: Glossy to satin
Color: White
Oribe Green
Firing Temperature: Cone 9-13
Atmosphere: Reduction, Oxidation/Neutral, Wood
Surface Finish: Satin to glossy
Color: Blue green