Mottled Purple
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Medium purple
Blue-Green/Copper Red Glaze
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Glossy
Color: Medium green, Medium red
Edgy Green
Firing Temperature: Cone 6
Atmosphere: Oxidation/Neutral
Surface Finish: Satin matte
Color: Turquoise green
Copper Red Luster
Firing Temperature: Cone 08
Atmosphere: Oxidation/Neutral
Surface Finish: Glossy
Color: Medium red
Willie Helix
Firing Temperature: Cone 10
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Matte
Color: Black
Reynold’s Gold Metallic Glaze
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation/Neutral
Surface Finish: Matte
Color: Gold
Patsy’s Green (Oribe)
Firing Temperature: Cone 10
Atmosphere: Oxidation/Neutral
Surface Finish: Matte
Color: Dark green