Vari-egated Green (Varigreen)
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Satin
Color: Green
Reynolds Green Metal Patina
Firing Temperature: Cone 6
Surface Finish: Satin
Color: Black
Opaque Matte #5
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Matte
Color: White, Blue
Ron Myers Clear
Firing Temperature: Cone 04-6
Atmosphere: Oxidation
Surface Finish: Glossy
Color: Clear, Red
Matt Kelleher Gloss
Firing Temperature: Cone 2–5
Atmosphere: Reduction, Oxidation
Surface Finish: Glossy
Color: Clear
Lisa Naples Earthenware Clay
Firing Temperature: Cone 1–2
Atmosphere: Oxidation
Color: Terra cotta
FLM Transfer Slip
Firing Temperature: Cone 9-10
Atmosphere: Reduction, Oxidation
Surface Finish: Matte to satin
Color: White
Miranda Thomas Jun Glaze
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Brown
Bill’s Basic Liner Glaze
Firing Temperature: Cone 04-2
Atmosphere: Oxidation
Surface Finish: Glossy
Color: White
Iron Slip
Firing Temperature: Cone 9
Atmosphere: Reduction, Wood
Surface Finish: Matte to satin
Color: Brown