Monroe New Zealand Casting Slip
Firing Temperature: Cone 6
Atmosphere: Reduction, Oxidation
Color: White
Lisa Naples Earthenware Clay
Firing Temperature: Cone 1–2
Atmosphere: Oxidation
Color: Terra cotta
Bates Clear
Firing Temperature: Cone 10
Atmosphere: Reduction, Oxidation
Surface Finish: Glossy
Color: Blue
Oriental Iron Glaze (3-A6-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Brown
Oriental Iron Glaze (3-A5-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Black, Brown
Oriental Iron Glaze (3-A4-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Brown
Oriental Iron Oxide (3-A3-R9)
Firing Temperature: Cone 9
Surface Finish: Glossy
Color: Brown
Oriental Iron Glaze (3-A1-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Blue
Flux Saturation (4-H4-O6)
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Satin matte
Color: Yellow
Flux Saturation (4-H3-O6)
Firing Temperature: Cone 6
Atmosphere: Oxidation
Surface Finish: Satin
Color: Yellow