Recipe Tags: Barium Carbonate (optional)

Chun Clear Turquoise

Chun Clear Turquoise

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Turquoise green

Chun Clear

Chun Clear

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Light green

Tony Hansen 20 x 5

Tony Hansen 20 x 5

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Reduction

Surface Finish: Satin matte

Color: Medium blue

Pinnell Celadon Revised

Pinnell Celadon Revised

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Reduction

Surface Finish: Matte

Color: Medium green