Peach Shino
Firing Temperature: Cone 10
Atmosphere: Reduction
Surface Finish: Glossy
Color: Shino
Shino Variation (2-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Satin
Color: Shino
Shino Variation (1-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Satin
Color: Brown
Oriental Iron Glaze (9-F4-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Matte to satin
Color: Medium green, Tan
Matte Flux Variation (4-D6-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Matte to satin
Color: Brown
Matte Flux Variation (4-D5-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Matte to satin
Color: Brown
Matte Flux Variation (4-D4-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Matte to satin
Color: Brown
Matte Flux Variation (4-D3-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Color: Tan
Matte Flux Variation (7-D5-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Satin
Color: Black
Matte Flux Variation (1-B2-R9)
Firing Temperature: Cone 9
Atmosphere: Reduction
Surface Finish: Glossy
Color: Blue