High Fire Glaze Recipes

High firing produces the most vitreous and durable ceramic work and many potters and ceramic artists choose to high fire for this very reason. And most artists who fire to this range mix their own glazes. Fortunately, many of them readily share their high fire glaze recipes with other potters and ceramic artists. In this section, you’ll find a collection of high fire glaze recipes, plus methods and techniques for firing in the high fire temperature range.

And don’t forget to download your free copy of 15 Tried and True Cone 10 Glaze Recipes: Recipe Cards for our Favorite High-Fire Pottery Glazes, a perfect resource for potters and ceramic artists who are ready to experiment with custom cone 10 glaze recipes, or for those who have grown tired of their own tried and true high fire glazes.

Although a lot of potters are reducing their firing temperatures these days, high-fired pottery is still going strong. Many contemporary potters are still creating traditional glaze surfaces with celadon glazes, oil spot glazes, and others. Whether you fire in oxidation, reduction, or neutral—with gas, electricity, or wood—you’ll find a wide variety of cone 10 glaze recipes (and above) with enormous possibilities for surfaces here in the archives.

Looking for reliable stoneware glaze recipes? We have everything from traditional Chun glaze recipes to ash glaze recipes that make use of ash right out of your fireplace! Is porcelain more your thing? We have that covered too. And, we don’t just have high fire glaze recipes. In addition to high fire glaze recipes, the artists share their techniques and advice for getting the most out of their high fire glaze formulas.

With this collection of information, you’ll discover that high fire does not mean high difficulty. So peruse through these pages and start experimenting with high fire glazes!

15+ Tried & True Cone 10 Glaze Recipes

Get more than 15 high-fire glaze recipes when you download this freebie15+ Tried & True Cone 10 Glaze Recipes.



Read More

Recipes: Atmospheric Glazes

1 Bottle and shot glass, to 8 in. (20 cm) in length, porcelain with Blue Salt glaze, 2015.

2 Plates, to 7 in. (18 cm) in length, porcelain, Bray Shino and Oxidation Celadon glazes, 2015.

3 Mug, 5 in. (13 cm) in height, porcelain, flashing slip, and Honey Celadon glaze, 2015.

4 Yunomi, 4 in. (10 cm) in height, porcelain,Yellow Salt glaze, 2015.

5 Pitcher and cup, 11 in. (23 cm) in height, porcelain, Green and Yellow Salt glazes, 2015. All pieces fired in a reduced wood/soda kiln fired to cone 10.

Lisa York shares some of the high-fire glaze and slip recipes she uses alone, in combination, and  … Read More